Assessing the root cause of a blade defect
A 2.0 MW V90 turbine, commissioned in 2008, experienced a shell debond from the boxbar...
D-TE™ – enabling operation through adverse conditions
A 1.7 MW wind turbine with 50.2 m blades suffered damage when approximately 0.5 m...
D-TE™ – restoring blade integrity for higher availability
Challenge A 5 MW wind turbine with 59.5 m blades, commissioned in 2013, was being...
D-String® enabling long-term performance with minimal repairs
A 1.5 MW wind turbine with 37 m blades, commissioned in 2007, had developed multiple...
D-TE™ – strengthening blades to withstand strong winds
A 0.9 MW wind turbine with 27 m blades, commissioned in 2012, was being curtailed...
D-String® + D-TE™ – custom solution to stop open trailing edge
A 1.5 MW wind turbine with 34 m blades, commissioned in 2003, was experiencing open...
D-TE™ – installation on 75 blades in South America
A 2.0 MW wind turbine, commissioned in 2014 with 47.5 m blades, was experiencing a...